Fractographic logging for determination of pre-core and core-induced fractures: Nicholas Combs No. 7239 well, Hazard, Kentucky

License(s):

Other (Open)

Methods results, and conclusions formulated during a prototype fractographic logging study of seventy-five feet of oriented Devonian shale core are summarized. The core analyzed is from the Nicholas Combs No. 7239 well located twelve miles due north of Hazard, Kentucky. The seventy-five foot core length was taken from a cored section lying between 2369.0 feet (subsea) and 2708.0 feet (subsea). Total core length is 339.0 feet. The core was extracted from the upper Devonian Ohio and Olentangy shale formations. Results indicate that there are few tectonic (pre-core) fractures within the studied core section. The region may nevertheless be cut at core sample depth by well-defined vertical or inclined tectonic fractures that the vertically drilled test core didn't intersect. This is likely since surface Plateau systematic fractures in other Plateau areas are vertical to sub-vertical and seldom have a frequency of less than one major fracture per foot. The remarkable directional preference of set three fractures about strikes of N 40/sup 0/ E, N 10/sup 0/ W, N 45/sup 0/ W, suggests some incipient pre-core rock anisotropy or stored directional strain energy. If this situation exists, the anisotropy strike change or stored strain variance from N 40/sup 0/ E to N 45/sup 0/ W downcore remains an unanswered question. Tectonic features, indicating local and/or regional movement plans, are present on and within the tectonic horizontal fracture set one. Slickensides had a preferred orientation within several core levels, and fibrous-nonfibrous calcite serves as fracture fillings.

Followers: 0

Citation (Click to Copy)

Data and Resources

    Gathering Resources...

Keywords

Additional Info

Field Value
Last Updated September 29, 2016, 16:41 (LMT)
Created September 29, 2016, 16:41 (LMT)
Citation Kulander, B.R.; Dean, S.L.; Barton, C.C. ---- Roy Long, Fractographic logging for determination of pre-core and core-induced fractures: Nicholas Combs No. 7239 well, Hazard, Kentucky, 2016-09-29, https://edx.netl.doe.gov/dataset/fractographic-logging-for-determination-of-pre-core-and-core-induced-fractures-nicholas-combs-no
Netl Product yes
Poc Email Roy.long@netl.doe.gov
Point Of Contact Roy Long
Program Or Project KMD
Publication Date 1977-1-1